Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.63 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.63 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S 796 M Colored ASA Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |