Polymer Property : Melt Flow = 9.44 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 9.44 g/10 min

@Load 2.16 kg,
Temperature 285 °C
9.44 g/10 min

@Load 4.76 lb,
Temperature 545 °F
Lehmann & Voss LUVOCOM® 1/CF/15/HS Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..