Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.00 - 82.0 g/10 min | 3.00 - 82.0 g/10 min | Average value: 27.0 g/10 min Grade Count:35 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |