Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.350 - 800 g/10 min | 0.350 - 800 g/10 min | Average value: 9.85 g/10 min Grade Count:193 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |