Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.70 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.70 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Synres® PP G15 18 Polypropylene, Glass Reinforced Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many .. |