Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.3 - 8.7 g/10 min @Load 5.00 kg, Temperature 372 °C |
4.3 - 8.7 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |