Polymer Property : Melt Flow = 8.64 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 8.64 g/10 min

@Load 10.0 kg,
Temperature 220 °C
8.64 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Terlux® 2812 HD MABS
Description: Terlux 2812 HD is a suitable grade for the food packaging and health care and diagnostic markets.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS