Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.55 g/10 min @Load 2.16 kg, Temperature 260 °C |
8.55 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238-10A |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |