Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.50 - 8.20 g/10 min | 4.50 - 8.20 g/10 min | Average value: 5.73 g/10 min Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |