Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.16 g/10 min | 8.16 g/10 min | JIS K7210 |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |