Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 79 g/10 min @Load 5.00 kg, Temperature 190 °C |
79 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 79 MFI
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel.. |
|||
Melt Flow | 79 g/10 min @Load 5.00 kg, Temperature 266 °C |
79 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 855 PBT (Europe-Africa-Middle East) VALOX 855 is 15% glass reinforced PBT+PET blend with improved surface appearance. Applications: external housings, steam irons, appliance housings and lighting parts. |
|||
Melt Flow | 79 g/10 min @Load 2.16 kg, Temperature 230 °C |
79 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, 50% RH Neat resin, for injection molding.Information provided by Cresset Powers Ltd. |
|||
Melt Flow | 79 g/10 min @Load 2.16 kg, Temperature 230 °C |
79 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Cresset Powers Cress-Alon™ A2350 2.35 r.v. Injection Molding Grade Nylon 6, Dry As Molded Neat resin, for injection molding.Information provided by Cresset Powers Ltd. |