Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 - 75.0 g/10 min | 1.00 - 75.0 g/10 min | Average value: 18.2 g/10 min Grade Count:44 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |