Physical Properties Metric English Comments
Melt Flow 2.00 - 73.8 g/10 min
2.00 - 73.8 g/10 min
Average value: 19.5 g/10 min Grade Count:22
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..