Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 7.15 g/10 min @Load 5.00 kg, Temperature 190 °C |
7.15 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |