Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 64.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
64.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Teijin Panlite® AD-5503 Optical Use Polycarbonate Resin High fluidity grade for optical media that provides low optical distortion moldings. Impurities in pellets are severely controlled, and resulting high quality is obtaining good reputation.Applicatio.. |