Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 64.2 g/10 min @Load 10.0 kg, Temperature 240 °C |
64.2 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Conditioned) Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur.. |
|||
Melt Flow | 64.2 g/10 min @Load 10.0 kg, Temperature 240 °C |
64.2 g/10 min @Load 22.0 lb, Temperature 464 °F |
ISO 1133 |
Styrolution Terblend® N NM-21 EF Gray 38058 ABS+PA (Dry) Description: Terblend® N NM-21 EF is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures. The enhanced flowability enables excellent processability and sur.. |