Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 62 g/10 min

@Load 2.16 kg,
Temperature 190 °C
62 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Chevron Phillips HiD® 9062 HDPE Injection Molding Resin  (discontinued **)
Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli..
Melt Flow 62 g/10 min

@Load 0.980 kg,
Temperature 190 °C
62 g/10 min

@Load 2.16 lb,
Temperature 374 °F
ASTM D1238
LyondellBasell Alathon® H4262 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ApplicationsAlathon H4262 is a high-flow resin that exhibits very good cold temperature impact performance, optimum processing and thermal stability, with good color and organoleptic properties. Typ..
Melt Flow 62 g/10 min

@Load 5.00 kg,
Temperature 250 °C
62 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT
Health care grade, PTFE and silicone lubricated
Melt Flow 62 g/10 min

@Load 10.0 kg,
Temperature 220 °C
62 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade
Very High Flow, Medium Impact GradeInformation provided by Bhansali
Melt Flow 62 g/10 min

@Load 10.0 kg,
Temperature 220 °C
62 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Bhansali Engineering Abstron IM-17A(HF) ABS Injection Molding Grade
Very High Flow, Medium Impact GradeInformation provided by Bhansali
Melt Flow 62 - 72 g/10 min

@Load 2.16 kg,
Temperature 235 °C
62 - 72 g/10 min

@Load 4.76 lb,
Temperature 455 °F
ASTM D1238
Gromax PBT 1200-211D
Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle..
Melt Flow 62 g/10 min

@Load 2.16 kg,
Temperature 190 °C
62 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 2915 HDPE Injection Molding Resin  (discontinued **)
Features: Excellent balance of stiffness and toughness, low odor, permits light weight container design.Applications: Thin walled food containers, frozen food containers.Data provided by the manufac..