Physical Properties Metric English Comments
Melt Flow 61 g/10 min

@Load 2.16 kg,
Temperature 260 °C
61 g/10 min

@Load 4.76 lb,
Temperature 500 °F
Calculated from MVR using melt density; ISO 1133
Lanxess Pocan® KU 2-7003 000000 PBT
PBT, non-reinforced, injection molding