Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.75 g/10 min @Load 2.16 kg, Temperature 230 °C |
6.75 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |