Physical Properties Metric English Comments
Melt Flow 59.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
59.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Conditioned)
Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles..
Melt Flow 59.2 g/10 min

@Load 5.00 kg,
Temperature 275 °C
59.2 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3GM35 BK 30564 15/25% Glass/Mineral Filled PA6 (Dry)
Description: 25% mineral-filled and 15% glass-fiber reinforced injection-molding grade for industrial articles having medium rigidity and high dimensional stability, used e.g. for covers and handles..