Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 550 g/10 min @Load 5.00 kg, Temperature 380 °C |
550 g/10 min @Load 11.0 lb, Temperature 716 °F |
|
Hybrid Plastics PK6U58.01 PEEK POSS® Flow Masterbatch POSS® Flow masterbatches have shown success in reducing the melt viscosity of a variety of high temperature, difficult to process, thermoplastics. Hybrid Plastics offers such a solution for PEEK... |