Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 54.4 g/10 min @Load 5.00 kg, Temperature 275 °C |
54.4 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Conditioned) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Melt Flow | 54.4 g/10 min @Load 5.00 kg, Temperature 275 °C |
54.4 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Melt Flow | 54.4 g/10 min @Load 5.00 kg, Temperature 275 °C |
54.4 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3WG6 BK 00564 30% Glass Filled PA66 (Conditioned) Description: 30% glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of high stiffness and dimensional stability such as lamp socket housings, f.. |