Polymer Property : Melt Flow = 522 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 522 g/10 min

@Pressure 0.655 MPa
522 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
PolyOne Geon™ 210 Series 217 Blending Resin Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 217 is a low to medium molecular weight homopolymer blending resin intended for use as a formulation tool in plastisol formulations.It improves air release performance resulting in reduced sc..