Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 52.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
52.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Conditioned)
Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V..
Melt Flow 52.5 g/10 min

@Load 2.16 kg,
Temperature 235 °C
52.5 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Dry)
Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V..