Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 50.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
50.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2235 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | >= 50.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
>= 50.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB2101 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 50.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
50.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2651A Thermoplastic Elastomer Uses: Flexible Grips; Footwear; General Purpose; Grommets; Handles; Industrial Applications; Soft Touch Applications; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed.. |