Physical Properties Metric English Comments
Melt Flow 5.72 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.72 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 4 cm<sup>3</sup>/10min.; ISO 1133
Mitsubishi Xantar® G6F 23 R Polycarbonate-30% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Melt Flow 5.72 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.72 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 4 cm<sup>3</sup>/10min.; ISO 1133
Mitsubishi Xantar® SF 2230 Polycarbonate-30% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Melt Flow 5.72 g/10 min

@Load 1.20 kg,
Temperature 300 °C
5.72 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 4 cm<sup>3</sup>/10min.; ISO 1133
Mitsubishi Xantar® G6F 23 UR Polycarbonate-30% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..