Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 - 5.00 g/10 min | 1.00 - 5.00 g/10 min | Average value: 3.00 g/10 min Grade Count:5 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |