Polymer Property : Melt Flow = 49.3 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 49.3 g/10 min

@Load 5.00 kg,
Temperature 275 °C
49.3 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Conditioned)
Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.
Melt Flow 49.3 g/10 min

@Load 5.00 kg,
Temperature 275 °C
49.3 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry)
Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability.