Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42 - 49 g/10 min @Load 2.16 kg, Temperature 235 °C |
42 - 49 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |