Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 470 g/10 min @Load 2.16 kg, Temperature 190 °C |
470 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 50E803 Anhydride Modified Polypropylene BYNEL® Series 5000 resins are anhydride-modified polypropylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polypropylen.. |