Physical Properties Metric English Comments
Melt Flow 39 - 47 g/10 min

@Load 2.16 kg,
Temperature 190 °C
39 - 47 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-00
Ipiranga Petrochem PRB 4215 Polypropylene
The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr..