Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 45.9 g/10 min @Load 1.20 kg, Temperature 300 °C |
45.9 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |