Melt Flow 42.9 g/10 min

@Load 2.16 kg,
Temperature 250 °C
42.9 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
BASF Ultradur® B 4560 PBT
Description: Medium viscosity injection molding grade for industrial parts in the automotive field, for example for head lamp bezel. Suitable for direct metalizing.Information provided by BASF