Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 400 g/10 min | 400 g/10 min | GB/T 3682-2000 |
Sichuan Deyang Haton® hc Polyphenylene Sulfide Resin Fiber gradeInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Melt Flow | 400 g/10 min @Load 2.16 kg, Temperature 190 °C |
400 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 210W Ethylene Vinyl Acetate DuPont™ Elvax® 210W is an ethylene-vinyl acetate copolymer resin containing an anti-blocking additive for use in industrial applications. This resin is supplied in pellet form and to prevent the p.. |
|||
Melt Flow | 400 g/10 min | 400 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ AD 0428EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 0428EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: .. |
|||
Melt Flow | 400 g/10 min | 400 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 40028CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 40028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |
|||
Melt Flow | 400 g/10 min | 400 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 40028EM1 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 40028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen.. |
|||
Melt Flow | 400 g/10 min @Load 2.16 kg, Temperature 190 °C |
400 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ UL 7711 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7711 is a very high flow, 26.7% VA copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making.. |
|||
Melt Flow | 400 g/10 min | 400 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ AD 0633EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 0433EH2 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: .. |
|||
Melt Flow | 400 g/10 min @Load 2.16 kg, Temperature 190 °C |
400 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont Elvax® 210 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 210 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 210 resins can be used for the following applications: adhesives, sealants,.. |