Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 40.2 g/10 min @Load 2.16 kg, Temperature 380 °C |
40.2 g/10 min @Load 4.76 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |