Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 380 g/10 min | 380 g/10 min | |
Solvay Specialty Polymers Ryton® P-6 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |