Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 37.7 g/10 min @Load 5.00 kg, Temperature 300 °C |
37.7 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2922 PPE (Asia Pacific) GF20% FR-V0 |