Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 36.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
36.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos T50-3600 HDPE Ineos T50-3600 is a high density polyethylene copolymer of narrow molecular weight distribution used primarily for high speed injection molding of thin-walled articles. It is characterized by a hig.. |
|||
Melt Flow | 36.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
36.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors. |
|||
Melt Flow | 36.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
36.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BMN D Nylon 11 (Conditioned) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
Melt Flow | 36.5 g/10 min @Load 2.16 kg, Temperature 235 °C |
36.5 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BMN D Nylon 11 (Dry) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |