Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 36.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
36.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® W2320 0035 POM Description: Is a POM, very free-flowing and rapidly solidifying grade for high processing demands.Information provided by BASF |