Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 34.84 g/10 min @Load 10.0 kg, Temperature 380 °C |
34.84 g/10 min @Load 22.0 lb, Temperature 716 °F |
6`; ASTM D1238 |
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |