Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 33.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
33.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® 6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin 6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont .. |
|||
Melt Flow | 33.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
33.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
DuPont Performance Polymers Crastin® FG6134 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Medium Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin® FG6134 NC010 is an unreinforced medium viscosity polybutylene terephthalate resin for injec.. |