Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 33.35 g/10 min @Load 2.16 kg, Temperature 250 °C |
33.35 g/10 min @Load 4.76 lb, Temperature 482 °F |
Calculated from Volume Flow Rate of 23 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnite® TV4 240 S PBT-20% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |