Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 31.97 g/10 min @Load 5.00 kg, Temperature 300 °C |
31.97 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50-1375 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |