Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 30.59 g/10 min @Load 2.16 kg, Temperature 275 °C |
30.59 g/10 min @Load 4.76 lb, Temperature 527 °F |
ISO 1133 |