Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.76 g/10 min

@Load 2.16 kg,
Temperature 250 °C
3.76 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133:1997
Nanocyl PLASTICYL™ PBT1501 Polybutylene Terephthalate with 3 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..