Polymer Property : Melt Flow = 3.617 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 3.617 g/10 min

@Load 5.00 kg,
Temperature 190 °C
3.617 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Microcell Composite Company CELLOMER® 2100 SBS Rubber Pellets
CELLOMER® PELLETS can be used in hot-pressing or with injection foaming boards. Featuring anti-slippage and elasticity.Information provided by Microcell Composite Company