Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 28.6 g/10 min @Load 2.16 kg, Temperature 250 °C |
28.6 g/10 min @Load 4.76 lb, Temperature 482 °F |
Calculated from Volume Flow Rate of 22 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnite® T06 200 (extrusion) PBT (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |