Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 270 g/10 min @Pressure 0.655 MPa |
270 g/10 min @Pressure 95.0 psi |
Severs Efflux; Geon® 1010 |
PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Melt Flow | 270 g/10 min @Pressure 0.655 MPa |
270 g/10 min @Pressure 95.0 psi |
Severs Efflux; Geon® 1010 |
PolyOne Geon™ 170 Series 179 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Melt Flow | 270 g/10 min @Load 5.00 kg, Temperature 316 °C |
270 g/10 min @Load 11.0 lb, Temperature 600 °F |
ASTM D1283 |
Chevron Phillips Ryton® PR33 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |