Physical Properties Metric English Comments
Melt Flow 27.9 g/10 min

@Load 2.16 kg,
Temperature 275 °C
27.9 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
BASF Ultradur® B 4040 G6 30% Glass Filled PBT + PET
PBT + PET, injection-molding grade containing 30% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin..