Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 27.8 g/10 min @Load 10.0 kg, Temperature 380 °C |
27.8 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |